Re-Enamel a Frame at Home

How two handbooks of 1913 and 1916 refinished a frame in the kitchen: the machine stripped and its fittings listed, the old enamel taken off, the tubes rubbed smooth and wiped, two brushed coats of enamel given plenty of time to dry, the wheels done last and the machine put together only when the enamel was hard. Every instruction is from the Ebykr archive; the drawings are Ebykr’s own.

DifficultyHardDust, patience and days of waiting (Ebykr’s estimate)
StepsSevenFrom Henry, 1913, and Cassell, 1916
You will needTen tools, six materialsThe list, in the sources’ terms
SourceHenry 1913 and Cassell 1916Records 94435 and 94257

Before you start

This page shows how period sources refinished a frame at home, step by step, in their own words and figures. It does not test or guarantee any repair. Cassell warns that caustic soda burns the skin, and the blowpipe, the turpentine and the enamel are fire risks. Ebykr adds one caution the sources do not give: paint on an old frame may contain lead, so ask a professional how to strip and dispose of it. Both books say a frame is better refinished or stove enameled by a trade enameller, and that plating and lining are not for the amateur.

On this page The drawing Tools and parts The steps in words What goes wrong Another way Sources

Escape also leaves this view.
    Drawing key
    Workbench view: one step at a time in large type, for a phone or tablet on the bench.

    Tools and parts

    In the sources’ own terms; every item is named in them. Tick each one off as you gather it.

    Tools

    • A brush and a blunt knife For the potash and for scraping (Henry, Cassell)
    • A putty knife Does well for the scraping (Henry)
    • A blowpipe or blow-lamp, and a wire brush Optional, for softening the enamel (Cassell)
    • Emery cloth in strips Coarse to fine, about 1 in. wide for the lugs (Henry, Cassell)
    • Clean linen rags Never a fluffy cotton rag (Cassell)
    • A flat camel-hair brush About 1 in. wide, one for each coat (Henry, Cassell)
    • A clean tin For the enamel (Henry, Cassell)
    • Pieces of wood To hold the frame by (Henry)
    • A wheel stand Two grooved pieces of wood on a board (Henry)
    • Hooks or wire To hang the frame to dry (Cassell)

    Both books name more (gold size for transfers, aluminum paint for a hub); those belong to the optional jobs.

    Parts and materials

    • Potash, or caustic soda A strong solution in water (Henry, Cassell)
    • Turpentine To wipe the frame and to clean the brushes (Henry, Cassell)
    • Plaster-of-paris To fill dents (Henry)
    • Enamel An air-drying enamel, or first-coating and finishing enamel (Henry, Cassell)
    • Varnish, and powdered pumice For the finish (Henry, Cassell)
    • Vaseline and sweet oil For the bearings and the polish (Henry)

    The steps in words

    The whole job, readable and printable without the drawing. Each step says what it rests on, and can take you back up to its drawing.

    Take the machine to pieces and list the parts

    Strip the machine of all its fittings and put the parts that need plating in a box by themselves. Take the bearing parts out, the bracket axle, the fork from the head and the spindles of the hubs and pedals, wrapping the balls from each part separately and marking where they belong. Henry makes two complete lists of the fittings, one pair of handles, chain wheel and cranks, two pedals, one headlock and so many nuts and bolts, sends one with the parts and keeps the other to check them when they come back. Plating is for a plater, the sources agree: if a hub has to be plated the spokes are cut out, and if a hub can be polished instead it is better to do that. Cassell says the frame, the forks, any mudguards and the wheels go to the enameler.

    What this step rests on
    • exact Two complete lists of the fittings, one sent and one kept to check them, and the cycle repairer’s signature for safety; the work of plating left to a plater; spokes cut out if a hub must be plated: Henry 1913, pages 76 and 77.
    • exact The machine stripped of all fittings, the plated parts in a box by themselves, the bearing parts, bracket axle, fork and spindles taken out and their balls wrapped separately and marked; a list of parts; the frame, forks, mudguards and wheels for enameling: Cassell 1916, pages 64 to 66.

    Take the old enamel off

    Henry makes a strong solution of potash in boiling water, puts it on the tubes with an old brush and scrapes with a blunt knife, a putty knife serving well, and calls it a tedious job. When the enamel is all off Henry finishes with strips of very coarse emery cloth about 1 in. wide, which get round the lugs. Cassell says many scrape the old enamel off with a blunt knife and emery, a slow process, and that it can be quicker with a brazing blowpipe or blow-lamp: heat about 1 ft. at a time until the enamel is soft and then scrape it off or use a wire brush, never heating a tube enough to make even the lightest one red. A chemical remover is possible but not usual: 1 lb. of common caustic soda to 1 gal. of water, put on hot, left a short time and washed off with hot water and a brush, with care that it does not touch the hands.

    What this step rests on
    • exact A strong solution of potash in boiling water put on with an old brush, the tubes scraped with a blunt or putty knife, then very coarse emery cloth strips about 1 in. wide round the lugs: Henry 1913, page 77.
    • exact Hot potash tanks in the trade; a blunt knife and emery, slow; a blowpipe or blow-lamp heating about 1 ft. at a time and a scraper or wire brush, the heat only enough to soften the enamel and never to redden the lightest tube; 1 lb. of caustic soda to 1 gal. of water, hot, washed off with hot water, harmful to the skin: Cassell 1916, page 66.
    • not stated Whether heat harms a tube: Cassell says it does not, if kept to softening the enamel, and a reader should weigh that for a frame of thin tubing.

    Rub the tubes smooth

    Cassell finishes with emery cloth when the parts are free of enamel and cooled, No. 2 or 2½ first and then FF or O, scouring the tubes lengthwise and finishing round the lugs with narrow strips used crosswise; for the best work the lugs are rubbed down with coarse and fine emery and ended with No. 1, and the lugs and sharp corners polished the lugs and sharp corners with strip emery. Henry says enamel cannot be applied properly to a scratchy surface, so the better the surface the better the result, and Henry fills any dents in the frame with plaster-of-paris. Dust the frame with a linen rag, never a fluffy cotton one, and dust out all holes and corners.

    What this step rests on
    • exact Emery cloth No. 2 or 2½, then FF or O, the tubes scoured lengthwise and the lugs finished crosswise with narrow strips: Cassell 1916, page 66.
    • exact The surface prepared as smooth as possible, since enamel cannot be applied properly to a scratchy one; dents filled with plaster-of-paris: Henry 1913, page 77.
    • exact The work rubbed down with coarse and fine emery and finished with No. 1, the lugs and corners polished with strip emery, dusted with a linen rag, never a fluffy cotton one, and all holes and corners dusted out: Cassell 1916, pages 72 and 73.
    • not stated The numbers of Cassell’s emery grades are the period’s own: no modern grit is given.

    Wipe it with turpentine and get the room ready

    Wipe the frame over with a clean rag dipped in turpentine, and after that do not handle it. If it has to be moved, drive pieces of wood into the down tube, the head and through the bottom bracket to hold it by. The room matters as much as the enamel: Cassell and Henry both want it warm and free from dust and draughts, Cassell adds clothes and tools free of dust, and both pick the kitchen, with a fire and the door shut. Use a good flat camel-hair brush about 1 in. wide, not a penny brush; Cassell keeps one for the first coat and another for the second, kept very clean. Pour a little enamel into a clean tin as it is wanted.

    What this step rests on
    • exact The frame wiped with a rag dipped in turpentine and then not handled; pieces of wood driven into the down tube, head and bottom bracket to shift it; a flat camel-hair brush about 1 in. wide; the kitchen, warm, free from dust and draught; enamel poured into a clean tin: Henry 1913, pages 78 and 79.
    • exact A room free from dust, cold and draughts, the workman’s clothes and the tools clean too; a flat camel-hair brush 1 in. or 1¼ in. wide, a separate brush for the first and the second coat, kept clean; the kitchen with a fire and the door shut: Cassell 1916, page 81.

    Give the first coat and let it dry

    Henry uses an air-drying enamel and gives the frame a good coat with long steady strokes, the brush kept moving in one direction and not loaded, or the enamel will run and look uneven. Cassell starts at the fork ends, inside the back forks and stays, then the down tube, the top and bottom tubes and the head, and wants a good even coat not so thick as to run. Hang the frame up to dry out of the way, with no tube quite horizontal. Allow plenty of time: Henry about 12 hours, Cassell 24 hours to dry and harden. Then look the work over for brush hairs and rough places and take them off before the second coat.

    What this step rests on
    • exact An air-drying enamel; long steady strokes in one direction, not too much on the brush, plenty of time for the first coat to dry, about twelve hours, then dusting and the second coat: Henry 1913, page 78.
    • exact The first coat started at the fork ends and worked toward the head, a good even coat not so thick as to run, the work hung up for 24 hours to dry and harden, brush hairs and rough places removed before the next coat: Cassell 1916, pages 82 and 83.
    • not stated The books give different drying times (about 12 hours and 24 hours), and neither gives a temperature for the room beyond “fairly warm”.

    Give the second coat and let it harden

    Dust the frame over with a clean rag and give the final coat, Henry says, and see that it is not too thick. Cassell lets the second coat dry as the first and examines it again for blemishes; if a little gold size or varnish is mixed with the flat color the surface can be rubbed down very lightly with powdered pumice on a damp cloth, and a finishing coat of varnish put on evenly with a good flow but not too thickly. Henry offers a thin coat of the best oak varnish to make the work more durable. Do not begin to put the machine together until the enamel is quite dry and hard: the longer it is left the better, Cassell says two or three days if possible, since the varnish is easily spoiled until it is really hard. Transfers go on before the varnish, and lining is a job for a professional.

    What this step rests on
    • exact The frame dusted and the final coat given; a thin coat of best oak varnish for durability; a transfer fixed with gold size when tacky, pressed from the center, moistened and peeled, then varnished; lining never attempted by the amateur: Henry 1913, pages 78 and 79.
    • exact The second coat dried and examined, gold size or varnish mixed in to allow a light rub with pumice on a damp cloth, a finishing coat of varnish evenly and not too thickly; the machine not assembled until the enamel is hard, two or three days if possible; transfers before varnishing, lining left to a professional: Cassell 1916, pages 82 and 83.
    • not stated Henry’s enamels (Chez Lui, Club Black, R.M.) and Cassell’s first-coating and finishing enamels are not the same, and none is named for today.

    Do the wheels, then put it together

    The wheels come last. Rub the spokes with emery cloth, and rub rust off the inside of the rim, which is fatal to the tires if left. Hold the wheel in a rough stand, or turned upside down in the frame, in which case do the wheels first. The spokes get one coat only, or they look thick and clumsy: Henry does the inside of the spokes first, working downward from the hub so that the enamel does not run on to it, and then the outside; Cassell begins at the crossing, goes round about 3 in. or 4 in. up, then from the nipples down to where the first left off, then reverses the wheel. The rim has two or even three coats, with the inside enameled as well. A rusty hub can be cleaned and given a coat of aluminum paint. When everything is hard, put the fittings back with the ball bearings in vaseline, adjust them and polish the frame with a soft rag, preferably old silk, and a little sweet oil.

    What this step rests on
    • exact The spokes rubbed with emery and given one coat only, the inside first working downward from the hub and then the outside; the rim two or three coats and the inside enameled to stop rust; a stand of two grooved pieces of wood; the fittings put back with vaseline and the frame polished with soft rag and sweet oil: Henry 1913, pages 79 and 80.
    • exact The spokes given one coat, from the crossing then from the nipples down, the wheel reversed, then the rim; the inside of the rims rubbed free of rust first; a rusty hub cleaned and given aluminum paint: Cassell 1916, pages 82 and 83.
    • exact The rims two or even three coats, the inside of the rim enameled; touching up for a chipped place: Henry 1913, pages 80 and 81.

    What goes wrong

    Each of these is a source’s own warning, except the last, which is what the sources leave out.

    • Dust and draughts Cassell says dust, cold or draughts are fatal to good work.
    • A coat too thick It runs and looks uneven (Henry); applied too freely it lumps (Cassell).
    • A scratchy surface Enamel cannot be applied properly to one (Henry).
    • Handling the frame Keep hands off after the turpentine wipe (Henry); a moist hand marks the work (Cassell).
    • Two coats on the spokes They look thick and clumsy: one coat only (Henry, Cassell).
    • Putting it together too soon The enamel is easily spoiled until hard, which takes some days (Cassell).
    • Caustic soda on the skin It has a powerful action on the skin (Cassell).
    • Amateur lining Nothing spoils a frame more than bad lining (Henry, Cassell).

    Safety and the finish of today Neither book mentions lead in old paint, the fumes of enamel or turpentine, or the filler and primer a frame would be given now. The enamels and the emery grades they name are not available as written.

    Related jobs

    Stove enameling by a trade enameller

    Both books say a frame sent stripped of all fittings to an enameller costs less. Cassell describes the trade way: first coat hung head downward and stoved one hour at 380° F., rubbed down with powdered pumice and water, a finishing coat hung fork ends down and stoved one and a quarter to one and a half hours, and hand-polished with pumice and rotten-stone for a glass-like surface. Cassell 1916, pages 74 and 75.

    Touching up chipped enamel

    Henry says a chipped place need not be re-enameled, since it can be touched up satisfactorily; Cassell says the patch should be blended so that there is no abrupt edge. Henry 1913, pages 80 and 81.

    Transfers and lining

    Henry puts a transfer on with a thin coat of gold size left to get tacky, presses it from the center and peels the paper after moistening it; both books say not to line a frame by hand, and Cassell describes sword pencils, gold size and gold leaf for the professional. Henry 1913, pages 79 and 80; Cassell 1916, pages 82 and 83.

    Sources

    Every record opens in the Ebykr archive. Each step above names the page it rests on.

    Record 94435, pages 75 to 81Peter Henry, Cycle Building and Repairing, 1913Chapter VI on cycle enameling: the fittings listed, the old enamel taken off with potash, the frame rubbed smooth, an air-drying enamel brushed on in two coats, transfers, the wheels and the polish.
    Record 94257, pages 64 to 66, 72 to 75 and 81 to 83Cassell, Cycle Repairing and Adjusting, 1916 reprintThe fittings taken off and listed, old enamel stripped by hand, blowpipe or caustic soda, the brushes and room, and enameling at home: coats, drying, wheels and spokes.

    Henry’s book is the Library of Congress copy on the Internet Archive; Cassell’s is DTU Library’s copy (Danmarks Tekniske Kulturarv). Both are public domain, and the archive carries their page images in full with Ebykr’s own reading of the print. The two agree on stripping, on a smooth surface, on a clean warm room and on two coats; they differ on the stripper, the drying time and the enamel. This page puts the sources in Ebykr’s own words and quotes nothing at length.

    Exact, derived and schematic

    • exactThe fittings listed and stripped; potash, blowpipe or caustic soda; emery grades; the turpentine wipe; the room and the brush; two coats and varnish with their drying times; one coat on the spokes, two on the rim; assembly when hard, vaseline and polish.
    • schematicThe drawing: the tube and lug, the brush, the flame, the clock, the wheel and its spokes, and all motion. Ebykr’s own drawing.
    • not statedLead in old paint, a modern enamel, fumes, the heat a thin tube can take, and a drying temperature.

    The Ebykr Digest

    A monthly letter on classic lightweight bicycles

    New articles, timelines, catalog finds and registry activity — assembled from the archive once a month. Your address is never shared.

    Double opt-in. One email per month. Unsubscribe at any time with one click.